The calculation principle of expansion is as follows

In the process of bending, there is tension stress in the outer layer and compression stress in the inner layer. From tension to compression, there is a transition layer neutral layer. The length of neutral layer remains the same after bending as before bending, so the neutral layer is the basis for calculating the unfolding length of bending parts. The position of neutral layer is related to the degree of deformation. When the bending radius (R angle shown in the figure below) is larger and the bending angle (θ angle shown in the figure below) increases, the degree of deformation increases, the position of neutral layer gradually moves to the inner side of the bending center, and the distance between neutral layer and inner layer of sheet metal is less than 90

Calculation method:

basic formula of expansion:

Expansion length = in stock + in stock + compensation

Development length = out of stock + out of stock – compensation

Right angle bending:

(R ≤ 2.0 θ = 90). L = a + B-K (see Table 2 for K value)

(R>2? ?θ=90)L=a+b+K

K=(R+λ)*π/2  

Note: when R ≥ 5T, λ = 0.5T

When R < 5T, λ = 0.4t

a. B is a direct boundary value tangent to R

A Post about Sheet Metal Processing Methods with Details 2

Obtuse angle bending:

( R≤2.0? ?θ>90):

L = a + B + (θ / 90) * k (see Table 1 for K value)

(R>2? θ>90 ):L=A+B+K?

 K=(R+λ)*πθ/180

注意:

When R ≥ 5T, λ = 0.5T

When R < 5T, λ = 0.4t

A. B is a straight boundary value tangent to R

A Post about Sheet Metal Processing Methods with Details 3

Acute bend:

2(R≠0   θ<90):

L=A+B+K  K=(R+λ)* πθ/180

注意:

When R ≥ 5T, λ = 0.5T

When R < 5T, λ = 0.4t

A. B is a straight boundary value tangent to R

A Post about Sheet Metal Processing Methods with Details 4

Z-fold (straight edge difference)

1. When h ≥ 4T, it is formed in two times and calculated according to two 90 bends.

2. When h < 4T, one-time molding.

L = a + B + K (see Table 3 for K value)

A Post about Sheet Metal Processing Methods with Details 5

Z-fold (bevel segment difference)

1. When h < 2T, it is calculated in the way of straight edge segment difference, i.e. L = D + K (see Table 3 for K value)

When h ≥ 2T, unfold by two-stage bending (θ≠ 90)

A Post about Sheet Metal Processing Methods with Details 6

Folding and flattening

1.L=A+B-0.4T

N fold

1. When the n-fold processing method is to fold and flatten the gasket, press

L = a + B + K. (see Table 4 for K value).

When n-fold is processed in other ways, it is calculated according to the general bending (R ≠ 0 θ≠ 90) “A Post about Sheet Metal Processing Methods with Details 7

A Post about Sheet Metal Processing Methods with Details 8
A Post about Sheet Metal Processing Methods with Details 9

design value of dimension with tolerance:

take the middle value of upper and lower limit dimension as design standard value

Pre opening bottom hole

In the process of unfolding, in addition to the shape unfolding, we need to take out teeth (flanging) tapping, tapping (extruding and cutting) flanging expanding riveting nuts (class Z products), flower tooth pressing riveting nuts (class s products), pressing riveting screws (class FH products) and pressing riveting screws (class NY products) Rivet nut column (so, BSO, soo, SOPC products) (pay attention to the difference between 3.5m3 and M3 bottom hole). In the process of unfolding, the bottom hole should be pre opened (see Table 5 for details)

Open process hole

For some products with low precision and need to be welded and polished, we can open a bending process hole at the bending corner. The size is determined by the plate thickness. It should be larger than the plate thickness, and it should not be too large. In the programming process, we should try to select the appropriate mold that has been used. (easy to reduce mold and processing time).A Post about Sheet Metal Processing Methods with Details 10

No process hole is needed for all the edge lapping relationships;

There are three kinds of graphs: all inclusive, half inclusive and edge overlapping.

For the thickness t < 1.5mm, there is no need to open the process hole;

If the plate thickness t ≥ 1.5mm with edge wrapping, the process hole shall be added at the corner.

There are two kinds of process holes: round and U-shaped; the center of the long round hole is on the bending line.

As shown in figure A.B

The expanded part is the part of line segment, which is processed into the form of process hole as shown in the figure below: as shown in Figure C

The width of process hole is 0.5 (laser) or 2.0 (NCT).

when the distance between the Extraction edge and the bending edge (inner dimension) is less than 2.0 mm, the bending process will be affected. At this time, the corresponding bending deformation area will be cut or the extraction dimension will be changed, as shown in Figure E

Under the following circumstances, it is not allowed to open process holes:

Parts with appearance or assembly relationship requirements and without customer’s permission;

Separate shipment, without the customer’s permission.

Japanese customers didn’t ask to start yikong:

2) In the following cases, the programmer can open the process hole at his own discretion:

the workpiece that needs to be welded and filled up in the next process after opening the angle of the process hole;

the workpiece that is not the appearance surface and does not affect the assembly and function, and is assembled inside the whole machine for shipment.

In the following cases, the Engineer shall negotiate with the customer to open the process hole

Work pieces that affect bending or die forming but have no process holes on the drawing.

All the parts without fillet (laser) after product development shall be rounded according to r0.5.

what do we do about hole around a bending edge

It is worth noting that when we find that there is a hole close to the bending edge in the process of unfolding, and the hole will bend after bending, we need to inform the engineer whether to open the bottom hole first and then expand the hole after bending. ?

There are two general formulas for reference

LMIN=(2.0-2.5)T+D/2 

L1 < V / 2 (V is V groove of lower die)

A Post about Sheet Metal Processing Methods with Details 11

Smooth surface and burr surface

in the process of unfolding, smooth surface and burr surface are one of the important contents that we must consider. Generally, for those not specified in the drawing and not specially required by customers, such as folding a box, we usually regard the inside as burr surface and the outside as smooth surface. For customers (such as Japanese customers such as VGI, TBS, Seiko, etc.), there are special requirements, which are clearly indicated in the drawings. We will carry out according to the requirements of the drawings.

Requirements for unfolding in folding machine processing

The general form of bending process of folding machine is shown in the attached figure. The selection of V groove is related to the material thickness, and its minimum hem size is limited by V groove. Its relationship is shown in the attached table

A Post about Sheet Metal Processing Methods with Details 12

Note: the minimum bending L in the table must be upper die with sharp knife;

The minimum h is Z-fold secondary molding (H ≥ 5T).

For Z-fold one-time forming (H ≤ 5T), the maximum length of Z-fold one-time forming is 835mm (2pcs), and there is no blocking in the middle.

The thickness of fault plate T: 0.5-2.3, the height of fault plate H: 0.5-10 mm.

Material saving placement: after the unfolding inspection is OK, we have to choose a reasonable placement method (generally x value > y value) to see how to place the most economical material, and rotate the unfolding drawing to a reasonable position (do not mirror, the burr surface will be reversed) And then arrange the knives.

コメントを殘す

メールアドレスが公開されることはありません。 が付いている欄は必須項(xiàng)目です

久久99国产综合精品女人-日韩一区二区三区在线不卡| 免费午夜福利在线观看-黄色日本黄色日本韩国黄色| 亚洲美女喘息呻吟的网站-国产免费一区二区三区三洲| 国产精品一区二区在线免费-久久精品国产亚洲av热明星| 久久人妻一区二区三区欧美-国内不卡的一区二区三区| 婷婷人妻少妇激情在线-欧美日韩人体艺术一区二区| 亚洲欧美另类综合偷拍-婷婷社区综合在线观看| 亚洲黑人欧美一区二区三区-亚洲一区二区三区免费视频播放| 中文字幕日韩精品不卡在线一区-国产tv日韩在线观看视频| 欧美日韩国产综合新一区-国产综合av一区二区三区| 欧美亚洲另类久久久精品-国产精品一区二区亚洲推荐| 国产av一区二区三区日韩接吻-av网址在线播放网站| 国产在线一区二区三区欧美-久久偷拍精品视频久久| 一区二区三区日本韩国欧美-日本1区2区3区4区在线观看| 99久久精品一区二区成人-麻豆国产av玩弄放荡人妇系列| 午夜福利卫生纸福利院-一区二区三区久久亚洲| 亚洲日本一区二区三区黄色电形-中文字幕乱码免费熟女| 91精品国产影片一区二区三区-欧美精品久久久精品一区二区| 日韩中文字幕v亚洲中文字幕-日韩亚洲av免费在线观看| av噜噜国产在线观看-欧美视频亚洲视频一区二区三区| 91精品国产影片一区二区三区-欧美精品久久久精品一区二区| 国产精品电影在线一区-亚洲国产大片一区二区官网| 91精品国产无线乱码在线-999精品视频免费看| 国产传媒中文字幕在线观看-午夜福利视频在线播放观看| 亚洲美女喘息呻吟的网站-国产免费一区二区三区三洲| 熟女少妇免费一区二区-麻豆一区二区三区免费在线观看| 熟女少妇免费一区二区-麻豆一区二区三区免费在线观看| 97人妻精品一区二区三区爱与-日韩精品亚洲专区在线观看| 国产日韩电影一区二区三区-美女露双奶头无遮挡物| 日本中文字幕啊啊啊啊-久久精品伊人久久精品伊人| 国产黄污网站在线观看-成人av电影中文字幕| 五月婷婷六月在线观看视频-亚洲黑寡妇黄色一级片| 欧美日韩亚洲1区2区-黄污视频在线观看不卡| 人妻日韩精品中文字幕图片-麻豆极度性感诱人在线露脸| 久久久噜噜噜久久狠狠50岁-精品一区二区三区av| 日韩二级视频在线观看-美女扒开奶罩露出奶子的视频网站| 天天干天天干2018-91人妻人人澡人爽精品| 国产精品久久99精品毛片-国产四季高清一区二区三区| av中文字幕男人天堂-懂色av一区二区三区在线观看| 国产一区二区三区噜噜-精品久久亚洲一区二区欧美| 免费看黄色污污的网站-欧美一区二区三区爽爽|